PRODUCT SPECIFICATION
TEST METHOD
|
Air Penetration Resistance
0.00082
ASTM E2178 (cfm/ft2@1.57 psf)
|
> 2500
Gurley Hill (TAPPI-T460) (sec/100cm)
|
Water Vapor Transmission
385
ASTM E96 Method A (g/m2/24 hrs)
|
|
465
ASTM E96 Method B (g/m2/24 hrs)
|
|
Water Penetration Resistance
> 300
AATCC 127 (cm)
|
Basis Weight
2.2
TAPPI T-410 (oz/sq yd)
|
Thickness
8
ASTM D3776 (mils)
|
Breaking Strength
30
ASTM D882 (lb/in) MD
|
|
Dry Tensile
45
ASTM D5034 (lb/in) MD
|
|
Tear Resistance (Trapezoid)
13.5
ASTM D1117 (lbs) MD
|
|
Drainage Efficiency
> 95%
ASTM E2273
|
> 95%
ICC-ES AC 235 Section 4.5
|
Surface Burning Characteristics
5 Class A
ASTM E84 Flame Spread Index
|
45 Class A
Smoke Develop Index
|
Ultra Violet Light Exposure
180 days
|